A Simplified Varestraint Test for Analyzing Weldability of Fe-Ni Based Superalloys

High temperature Ni-based superalloys are largely used in components of aircraft engines which are subjected to high thermal (above 700 °C) and structural loads. Investment casting has been traditionally implemented for the manufacturing of these components with different levels of complexity and size. However, investment casting of large and complex parts can entail some difficulties which lead to higher casting defect ratios and the need of repairing. Therefore, it is essential to develop easy to repair Ni-based superalloys castings, i.e., castings with an enhanced weldability or reduced weld cracking susceptibility. Improvement of weldability will also enable the combination of small size castings with forged and rolled components in welded structures reducing overall manufacturing costs and foundry capacity requirements. Cracking susceptibility of Ni-based superalloy castings is much greater in comparison with equivalent wrought components due to coarser and non-homogeneous microstructures, grain boundary segregations and particular chemistry which promote several cracking mechanisms during welding. A methodology based on Varestraint test (hot cracking test) is introduced to evaluate cracking susceptibility of Ni-based superalloys with a reduced number of samples. This reduction is particularly important when considering castings since practical conclusions can be drawn with minimum material usage. Influence of Varestraint testing parameters, machine performance and total crack length (TCL) measurement procedure on scattering of results are assessed. Conditions to reduce scattering and improve repeatability as well as reproducibility of results are defined, which are essential to compare weldability performance between different alloys and microstructures..

Authors:

P. Alvarez (LORTEK), L. Vázquez (LORTEK), P. M. García-Riesco (LORTEK), P. P. Rodríguez (Alfalan), Ana Magaña (AZTERLAN), Fernando Santos (AZTERLAN).

Keywords:

Ni-based superalloys, Weldability, Hot cracking, Varestraint, Solidification cracking, HAZ cracking.

Back

How can we help you?.

Keep up with AZTERLAN’s activity.

Fill out this form to download this resource

Request demo

Fill out this form to receive access to demo contents of the course in your email. 

Contact Gorka

Get in touch with Andoni

Contacta con Ramón

Contacta con Xabier

Contact with Maider Muro

Contact with Dr. Urko de la Torre

Contact with Dra. Anna Regordosa

Contact with Aitor Loizaga

Contact with Dr. Rodolfo González-Martínez

Contact Ander.

Contact with David Aristondo.

Contact with Juan J. Bravo.

Contact with David Garcia.

Contact with Jose Ramon.

Contact with Oihana.

Keep up with AZTERLAN’s activity.

Contact with David.

Contact with Ibon.

Contact with Hegoi.

Contact with Itziar.

Contact with Erika.

Contact with Beñat.

Contact with John.

Contact José Javier.